**Author:** ![andrey\_198](https://forum.idryer.org/letter_avatar_proxy/v4/letter/a/3be4f8/32.png) [@andrey\_198](https://forum.idryer.org/u/andrey_198)\
**Post date:** [February 27, 2026, 12:04pm UTC](https://forum.idryer.org/t/which-plastic-to-choose-for-the-enclosure-regular-abs-or-abs-gf/1699/1 "2026-02-27T12:04:36Z")

</div>

What plastic would you recommend for the case? Default is ABS, but since I don’t have a blower fan yet, there’ll probably be issues with ABS. Maybe some ABS-based composite?

> **🇷🇺 Оригинал**
>
> Какой пластик посоветуете для корпуса ? Дефолт - АБС, но пока дуйки нет - будут наверно проблемы с АБС. Может какой композит на основе АБС ?

---

<div class="post-metadata">

**Author:** ![justolik\_463](https://forum.idryer.org/letter_avatar_proxy/v4/letter/j/8e8cbc/32.png) [@justolik\_463](https://forum.idryer.org/u/justolik_463)\
**Post date:** [February 27, 2026, 12:19pm UTC](https://forum.idryer.org/t/which-plastic-to-choose-for-the-enclosure-regular-abs-or-abs-gf/1699/2 "2026-02-27T12:19:25Z")

</div>

ABS prints well just in an enclosed chamber. Besides, the bed warms it up pretty well. It’s just a matter of time. Print with a thinner layer, then the layer bonding is pretty good even without heating the chamber. The main thing is no drafts.

> **🇷🇺 Оригинал**
>
> Абс хорошо печатается просто в закрытой камере. К тому же стол неплохо её прогревает. Вопрос времени. Печатай слоем потоньше, тогда спекаемость неплохая и без прогрева камеры. Главное без сквозняков

---

<div class="post-metadata">

**Author:** ![ilya\_borisov\_480](https://forum.idryer.org/letter_avatar_proxy/v4/letter/i/5f9b8f/32.png) [@ilya\_borisov\_480](https://forum.idryer.org/u/ilya_borisov_480)\
**Post date:** [February 27, 2026, 12:26pm UTC](https://forum.idryer.org/t/which-plastic-to-choose-for-the-enclosure-regular-abs-or-abs-gf/1699/3 "2026-02-27T12:26:12Z")

</div>

Regular ABS. Just an enclosed chamber is fine, before printing you heat the chamber up to about 48-50 degrees, set the bed to max and about 5-10% side cooling, once you see 48 in the chamber, start the print.

> **🇷🇺 Оригинал**
>
> Обычный АБС. Просто закрытая камера норм, перед печатью камеру прогреваешь градусов до 48-50, ставишь стол на максимум и процентов 5-10 боковой обдув, увидел значение 48 в камере, запускаешь печать

---

<div class="post-metadata">

**Author:** ![andrey\_kekht\_ko\_b5c0](https://forum.idryer.org/letter_avatar_proxy/v4/letter/a/9de053/32.png) [@andrey\_kekht\_ko\_b5c0](https://forum.idryer.org/u/andrey_kekht_ko_b5c0)\
**Post date:** [February 27, 2026, 12:34pm UTC](https://forum.idryer.org/t/which-plastic-to-choose-for-the-enclosure-regular-abs-or-abs-gf/1699/4 "2026-02-27T12:34:14Z")

</div>

well that’s the meta then (what the ones in the doc photos are printed from) - Fusrock ABS GF

> **🇷🇺 Оригинал**
>
> ну так мета же (из чего напечатаны те что на фотках в доке) - Fusrock ABS GF